AIM: To evaluate the bonding durability of materials used as sealants on different dentitions. METHODS: Deciduous (D) and permanent (P) molars were divided into four groups (n=5) and sealed with Fluroshield (F) and OptiBond FL (FL). Blocks of composite resin were built, stored in distilled water (24 h/37 °C), sectioned into 0.8 mm2 and tested at tensile (0.5 mm/min) after 24 h and 6 months. The fractures were observed and classified into adhesive, cohesive or mixed types. The data were analyzed using repeated measures ANOVA and Tukey test (α=5%), with tooth as the experimental unit. RESULTS: There were differences for dentition (p=0.0097), dental sealant (p=0.0019) and time (p=0.0001). At 24h the highest bond strength was observed for OptiBond FL on deciduous and permanent teeth, similar to Fluroshield at both dentitions. After 6 months the bond strength of OptiBond FL did not decrease in the permanent teeth, but decreased similar to Fluroshield in deciduous teeth, the bond strength of Fluroshield decreased similarly in both dentitions. CONCLUSIONS: The bond strength of dental sealants varied with the experimental conditions.

Saved in:
Bibliographic Details
Main Authors: Moura,Sandra Kiss, Lemos,Letícia Vargas Freire Martins, Myszkovisk,Suellen, Provenzano,Maria Gisette Arias, Balducci,Ivan, Myaki,Silvio Issao
Format: Digital revista
Language:English
Published: Faculdade de Odontologia de Piracicaba - UNICAMP 2014
Online Access:http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1677-32252014000300198
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:AIM: To evaluate the bonding durability of materials used as sealants on different dentitions. METHODS: Deciduous (D) and permanent (P) molars were divided into four groups (n=5) and sealed with Fluroshield (F) and OptiBond FL (FL). Blocks of composite resin were built, stored in distilled water (24 h/37 °C), sectioned into 0.8 mm2 and tested at tensile (0.5 mm/min) after 24 h and 6 months. The fractures were observed and classified into adhesive, cohesive or mixed types. The data were analyzed using repeated measures ANOVA and Tukey test (α=5%), with tooth as the experimental unit. RESULTS: There were differences for dentition (p=0.0097), dental sealant (p=0.0019) and time (p=0.0001). At 24h the highest bond strength was observed for OptiBond FL on deciduous and permanent teeth, similar to Fluroshield at both dentitions. After 6 months the bond strength of OptiBond FL did not decrease in the permanent teeth, but decreased similar to Fluroshield in deciduous teeth, the bond strength of Fluroshield decreased similarly in both dentitions. CONCLUSIONS: The bond strength of dental sealants varied with the experimental conditions.