Recuperação de metais de catalisadores usados de hidrotratamento (NiMo E CoMo/AL2O3)

This work presents a detailed study of the leaching behavior of deactivated hydrotreating catalysts (CoMo, NiMo/Al2O3) in presence of oxalate and NH4+ ions in various media. The yield of metals recovery may be optimized by adjusting several experimental parameters (time, temperature, etc). Leaching is limited by physical factors (diffusional effects caused by coke) and by the existence of silicate/spinel-like species which are poorly soluble in leaching solutions. Coke may be eliminated by an oxidation step at temperatures between 300-400ºC. Above 400ºC, solubilization of Ni and Co is drastically reduced. 50-90% wt of sulphate species and 15-30% wt of phosphate ions are solubilized during leaching. Silicon (as SiO2) is not solubilized. The best Ni-Co-Mo recoveries are in the 70-90% wt range; Fe recovery may be quantitative, whereas Al leaching may be lower than 5% wt.

Saved in:
Bibliographic Details
Main Authors: Afonso,Júlio C., Lajter,Karen, Góes,Ronny S.
Format: Digital revista
Language:Portuguese
Published: Sociedade Brasileira de Química 1997
Online Access:http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40421997000400002
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:This work presents a detailed study of the leaching behavior of deactivated hydrotreating catalysts (CoMo, NiMo/Al2O3) in presence of oxalate and NH4+ ions in various media. The yield of metals recovery may be optimized by adjusting several experimental parameters (time, temperature, etc). Leaching is limited by physical factors (diffusional effects caused by coke) and by the existence of silicate/spinel-like species which are poorly soluble in leaching solutions. Coke may be eliminated by an oxidation step at temperatures between 300-400ºC. Above 400ºC, solubilization of Ni and Co is drastically reduced. 50-90% wt of sulphate species and 15-30% wt of phosphate ions are solubilized during leaching. Silicon (as SiO2) is not solubilized. The best Ni-Co-Mo recoveries are in the 70-90% wt range; Fe recovery may be quantitative, whereas Al leaching may be lower than 5% wt.