Strength of 3Y-TZP and feldspathic porcelain subjected to different cooling methods
AIM: To investigate the effect of the cooling rate on flexural strength of monolayer and bilayer porcelain/zirconia (Y-TZP) bars.METHODS: Forty-five specimens were made for each design group: (PM) monolithic specimens of veneer porcelain Vita VM9 (Vita, Germany); (ZM) monolithic specimens of zirconia (ZiHP; ProtMat, Brazil); (PB) bilayer specimens zirconia/porcelain with porcelain on lower surface; and (ZB) bilayer specimens porcelain/zirconia with zirconia on lower surface. Each group was cooled by three different methods after porcelain sintering: slow specimens were cooled inside the turned-off furnace; normal specimens were removed from the furnace and cooled in air at room temperature; and fast specimens were removed from the furnace at 910°C and cooled by compressed air for 10 s. Specimens were polished and flexural strength was measured in water at 37 °C (n=15). Maximum load at fracture was recorded, and equations for simple (monolayer) and composite (bilayer) structures were used to calculate the flexural strength. RESULTS were analyzed using one-way ANOVA (p<0.05) and Tukey test separately for each design.RESULTS: The results of one-way ANOVA were statistically significant only for the PB group. The post-hoc Tukey test showed the highest flexural strength for fast cooling and the lowest for slow cooling; the normal cooling was statistically similar to both.CONCLUSIONS: Cooling methods affected only the flexural strength of bilayer specimens with porcelain on low surface (under tension) when the slow cooling method was used.
Main Authors: | , , , , |
---|---|
Format: | Digital revista |
Language: | English |
Published: |
Faculdade de Odontologia de Piracicaba - UNICAMP
2014
|
Online Access: | http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1677-32252014000200124 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|