The use of a graphite-silicone rubber composite electrode in the determination of rutin in pharmaceutical formulation

The possibility of using a graphite silicone-rubber composite electrode (GSR) in a differential pulse voltammetric(DPV) procedure for rutin (vitamin P) determination is described. Cyclic voltammograms of rutin presented a reversible pair of oxidation/reduction peaks respectively at 0.411 and 0.390 V (vs. SCE) at the GSR surface in Britton-Robinson(B-R) buffer solution pH 4.0. In DPV after optimization of conditions, an oxidation peak at 0.370 V (vs. SCE) was used to quantitative determination of rutin in B-R buffer solution pH 4.0. In this case a linear dynamic range of 5.0×10-8 to 50.0×10-8 mol L-1 was observed with a detection limit of 1.8×10-8 mol L-1 for the analyte. Recoveries from 94 to 113% were observed. The electrode surface was renewed by polishing after each determination, with a repeatability of 1.09 ± 0.06 µA (n = 10) peak current. Rutin was determined in a pharmaceutical formulation using the proposed electrode and the results agreed with those from an official method within 95% confidence level.

Saved in:
Bibliographic Details
Main Authors: Santos,Sidney X. dos, Mazo,Luiz H., Cavalheiro,Éder T. G.
Format: Digital revista
Language:English
Published: Sociedade Brasileira de Química 2008
Online Access:http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0103-50532008000800021
Tags: Add Tag
No Tags, Be the first to tag this record!