Volume loss as a tool to assess kiln drying of eucalyptus wood
In this study, we aimed to analyze the kiln drying quality of Eucalyptus grandis, Eucalyptus saligna and Eucalyptus dunnii woods with respect to volume loss. Wood from the three species was kiln dried together with the same drying schedule and conditions in a conventional-temperature pilot kiln. Three kinds of volume loss were evaluated: total - from saturated (initial) to machined (final) condition; shrinkage - from saturated to 10% moisture content; and machining - from 10% moisture content to machined condition. Eucalyptus grandis wood was the most dimensionally stable and presented the smallest volume loss due to shrinkage. Although they had different shrinkage behaviors, Eucalyptus grandis and Eucalyptus saligna woods presented the same drying quality regarding machining and total volume losses. These species can be considered the same for kiln drying. Eucalyptus dunnii wood presented the worst quality in drying, and should not be kiln dried in the same batch with the other species.
Main Authors: | , , , , |
---|---|
Format: | Digital revista |
Language: | English |
Published: |
Instituto de Florestas da Universidade Federal Rural do Rio de Janeiro
2013
|
Online Access: | http://old.scielo.br/scielo.php?script=sci_arttext&pid=S2179-80872013000200013 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|