Adhesive systems used for sealing contaminated surfaces: a microleakage evaluation
The aim of this study was to compare two adhesive systems (OptiBond FL TM and OptiBond SOLO TM) used as a sole material for sealing pit and fissures on contaminated surfaces with respect to microleakage. After acid etching, 56 sound teeth were contaminated with 1 µl of plasma and randomly divided into 8 groups (n = 7). The adhesives were light activated under two conditions (Optilux VCL-403TM and VCL-500TM) for 30 s. Each specimen was exposed to one of the following aging treatments: thermal (4,000 X at 5-55°C for 60 s) plus load cycling (225,000 X with 83.3 N) or thermal plus load and pH cycling (mineralizing/demineralizing solutions). Then, they were immersed in a 50% AgNO3 aqueous solution, sectioned twice and had dye penetration measured through digitized images. ANOVA methods were used to assess the main effects of the factors as well as their interactions. The results indicated a significant difference between the adhesive systems (p < 0.05), suggesting that OptiBond FL TM has a better performance with respect to microleakage and could be used as a sealing material in accidentally moist or contaminated surfaces.
Main Authors: | , , , , , |
---|---|
Format: | Digital revista |
Language: | English |
Published: |
Sociedade Brasileira de Pesquisa Odontológica - SBPqO
2005
|
Online Access: | http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1806-83242005000100004 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
id |
oai:scielo:S1806-83242005000100004 |
---|---|
record_format |
ojs |
spelling |
oai:scielo:S1806-832420050001000042005-06-22Adhesive systems used for sealing contaminated surfaces: a microleakage evaluationGrande,Rosa Helena MirandaReis,AlessandraLoguercio,Alessandro DouradoSinger,Julio da MottaShellard,EdwardChristino Neto,Paulo Dentin-bonding agents Dental enamel Dental leakage Pit and fissure sealants The aim of this study was to compare two adhesive systems (OptiBond FL TM and OptiBond SOLO TM) used as a sole material for sealing pit and fissures on contaminated surfaces with respect to microleakage. After acid etching, 56 sound teeth were contaminated with 1 µl of plasma and randomly divided into 8 groups (n = 7). The adhesives were light activated under two conditions (Optilux VCL-403TM and VCL-500TM) for 30 s. Each specimen was exposed to one of the following aging treatments: thermal (4,000 X at 5-55°C for 60 s) plus load cycling (225,000 X with 83.3 N) or thermal plus load and pH cycling (mineralizing/demineralizing solutions). Then, they were immersed in a 50% AgNO3 aqueous solution, sectioned twice and had dye penetration measured through digitized images. ANOVA methods were used to assess the main effects of the factors as well as their interactions. The results indicated a significant difference between the adhesive systems (p < 0.05), suggesting that OptiBond FL TM has a better performance with respect to microleakage and could be used as a sealing material in accidentally moist or contaminated surfaces.info:eu-repo/semantics/openAccessSociedade Brasileira de Pesquisa Odontológica - SBPqOBrazilian Oral Research v.19 n.1 20052005-03-01info:eu-repo/semantics/articletext/htmlhttp://old.scielo.br/scielo.php?script=sci_arttext&pid=S1806-83242005000100004en10.1590/S1806-83242005000100004 |
institution |
SCIELO |
collection |
OJS |
country |
Brasil |
countrycode |
BR |
component |
Revista |
access |
En linea |
databasecode |
rev-scielo-br |
tag |
revista |
region |
America del Sur |
libraryname |
SciELO |
language |
English |
format |
Digital |
author |
Grande,Rosa Helena Miranda Reis,Alessandra Loguercio,Alessandro Dourado Singer,Julio da Motta Shellard,Edward Christino Neto,Paulo |
spellingShingle |
Grande,Rosa Helena Miranda Reis,Alessandra Loguercio,Alessandro Dourado Singer,Julio da Motta Shellard,Edward Christino Neto,Paulo Adhesive systems used for sealing contaminated surfaces: a microleakage evaluation |
author_facet |
Grande,Rosa Helena Miranda Reis,Alessandra Loguercio,Alessandro Dourado Singer,Julio da Motta Shellard,Edward Christino Neto,Paulo |
author_sort |
Grande,Rosa Helena Miranda |
title |
Adhesive systems used for sealing contaminated surfaces: a microleakage evaluation |
title_short |
Adhesive systems used for sealing contaminated surfaces: a microleakage evaluation |
title_full |
Adhesive systems used for sealing contaminated surfaces: a microleakage evaluation |
title_fullStr |
Adhesive systems used for sealing contaminated surfaces: a microleakage evaluation |
title_full_unstemmed |
Adhesive systems used for sealing contaminated surfaces: a microleakage evaluation |
title_sort |
adhesive systems used for sealing contaminated surfaces: a microleakage evaluation |
description |
The aim of this study was to compare two adhesive systems (OptiBond FL TM and OptiBond SOLO TM) used as a sole material for sealing pit and fissures on contaminated surfaces with respect to microleakage. After acid etching, 56 sound teeth were contaminated with 1 µl of plasma and randomly divided into 8 groups (n = 7). The adhesives were light activated under two conditions (Optilux VCL-403TM and VCL-500TM) for 30 s. Each specimen was exposed to one of the following aging treatments: thermal (4,000 X at 5-55°C for 60 s) plus load cycling (225,000 X with 83.3 N) or thermal plus load and pH cycling (mineralizing/demineralizing solutions). Then, they were immersed in a 50% AgNO3 aqueous solution, sectioned twice and had dye penetration measured through digitized images. ANOVA methods were used to assess the main effects of the factors as well as their interactions. The results indicated a significant difference between the adhesive systems (p < 0.05), suggesting that OptiBond FL TM has a better performance with respect to microleakage and could be used as a sealing material in accidentally moist or contaminated surfaces. |
publisher |
Sociedade Brasileira de Pesquisa Odontológica - SBPqO |
publishDate |
2005 |
url |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1806-83242005000100004 |
work_keys_str_mv |
AT granderosahelenamiranda adhesivesystemsusedforsealingcontaminatedsurfacesamicroleakageevaluation AT reisalessandra adhesivesystemsusedforsealingcontaminatedsurfacesamicroleakageevaluation AT loguercioalessandrodourado adhesivesystemsusedforsealingcontaminatedsurfacesamicroleakageevaluation AT singerjuliodamotta adhesivesystemsusedforsealingcontaminatedsurfacesamicroleakageevaluation AT shellardedward adhesivesystemsusedforsealingcontaminatedsurfacesamicroleakageevaluation AT christinonetopaulo adhesivesystemsusedforsealingcontaminatedsurfacesamicroleakageevaluation |
_version_ |
1756431448073568256 |