Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials

Objectives This study aimed to compare the micro-tensile bond strength of methacrylate resin systems to a silorane-based restorative system on dentin after 24 hours and six months water storage. Material and Methods The restorative systems Adper Single Bond 2/Filtek Z350 (ASB), Clearfil SE Bond/Z350 (CF), Adper SE Plus/Z350 (ASEP) and P90 Adhesive System/Filtek P90 (P90) were applied on flat dentin surfaces of 20 third molars (n=5). The restored teeth were sectioned perpendicularly to the bonding interface to obtain sticks (0.8 mm2) to be tested after 24 hours (24 h) and 6 months (6 m) of water storage, in a universal testing machine at 0.5 mm/min. The data was analyzed via two-way Analysis of Variance/Bonferroni post hoc tests at 5% global significance. Results Overall outcomes did not indicate a statistical difference for the resin systems (p=0.26) nor time (p=0.62). No interaction between material × time was detected (p=0.28). Mean standard-deviation in MPa at 24 h and 6 m were: ASB 31.38 (4.53) and 30.06 (1.95), CF 34.26 (3.47) and 32.75 (4.18), ASEP 29.54 (4.14) and 33.47 (2.47), P90 30.27 (2.03) and 31.34 (2.19). Conclusions The silorane-based system showed a similar performance to methacrylate-based materials on dentin. All systems were stable in terms of bond strength up to 6 month of water storage.

Saved in:
Bibliographic Details
Main Authors: SAMPAIO,Renata Kirita Doi, WANG,Linda, CARVALHO,Rodrigo Varella de, GARCIA,Eugenio José, ANDRADE,Andréa Mello de, KLEIN-JÚNIOR,Celso Afonso, GRANDE,Rosa Helena Miranda, MOURA,Sandra Kiss
Format: Digital revista
Language:English
Published: Faculdade De Odontologia De Bauru - USP 2013
Online Access:http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1678-77572013000100080
Tags: Add Tag
No Tags, Be the first to tag this record!
id oai:scielo:S1678-77572013000100080
record_format ojs
spelling oai:scielo:S1678-775720130001000802016-09-16Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materialsSAMPAIO,Renata Kirita DoiWANG,LindaCARVALHO,Rodrigo Varella deGARCIA,Eugenio JoséANDRADE,Andréa Mello deKLEIN-JÚNIOR,Celso AfonsoGRANDE,Rosa Helena MirandaMOURA,Sandra Kiss Dentin Bonding Dental adhesives Composite resins Longevity Objectives This study aimed to compare the micro-tensile bond strength of methacrylate resin systems to a silorane-based restorative system on dentin after 24 hours and six months water storage. Material and Methods The restorative systems Adper Single Bond 2/Filtek Z350 (ASB), Clearfil SE Bond/Z350 (CF), Adper SE Plus/Z350 (ASEP) and P90 Adhesive System/Filtek P90 (P90) were applied on flat dentin surfaces of 20 third molars (n=5). The restored teeth were sectioned perpendicularly to the bonding interface to obtain sticks (0.8 mm2) to be tested after 24 hours (24 h) and 6 months (6 m) of water storage, in a universal testing machine at 0.5 mm/min. The data was analyzed via two-way Analysis of Variance/Bonferroni post hoc tests at 5% global significance. Results Overall outcomes did not indicate a statistical difference for the resin systems (p=0.26) nor time (p=0.62). No interaction between material × time was detected (p=0.28). Mean standard-deviation in MPa at 24 h and 6 m were: ASB 31.38 (4.53) and 30.06 (1.95), CF 34.26 (3.47) and 32.75 (4.18), ASEP 29.54 (4.14) and 33.47 (2.47), P90 30.27 (2.03) and 31.34 (2.19). Conclusions The silorane-based system showed a similar performance to methacrylate-based materials on dentin. All systems were stable in terms of bond strength up to 6 month of water storage.info:eu-repo/semantics/openAccessFaculdade De Odontologia De Bauru - USPJournal of Applied Oral Science v.21 n.1 20132013-02-01info:eu-repo/semantics/articletext/htmlhttp://old.scielo.br/scielo.php?script=sci_arttext&pid=S1678-77572013000100080en10.1590/1678-7757201302329
institution SCIELO
collection OJS
country Brasil
countrycode BR
component Revista
access En linea
databasecode rev-scielo-br
tag revista
region America del Sur
libraryname SciELO
language English
format Digital
author SAMPAIO,Renata Kirita Doi
WANG,Linda
CARVALHO,Rodrigo Varella de
GARCIA,Eugenio José
ANDRADE,Andréa Mello de
KLEIN-JÚNIOR,Celso Afonso
GRANDE,Rosa Helena Miranda
MOURA,Sandra Kiss
spellingShingle SAMPAIO,Renata Kirita Doi
WANG,Linda
CARVALHO,Rodrigo Varella de
GARCIA,Eugenio José
ANDRADE,Andréa Mello de
KLEIN-JÚNIOR,Celso Afonso
GRANDE,Rosa Helena Miranda
MOURA,Sandra Kiss
Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
author_facet SAMPAIO,Renata Kirita Doi
WANG,Linda
CARVALHO,Rodrigo Varella de
GARCIA,Eugenio José
ANDRADE,Andréa Mello de
KLEIN-JÚNIOR,Celso Afonso
GRANDE,Rosa Helena Miranda
MOURA,Sandra Kiss
author_sort SAMPAIO,Renata Kirita Doi
title Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
title_short Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
title_full Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
title_fullStr Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
title_full_unstemmed Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
title_sort six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
description Objectives This study aimed to compare the micro-tensile bond strength of methacrylate resin systems to a silorane-based restorative system on dentin after 24 hours and six months water storage. Material and Methods The restorative systems Adper Single Bond 2/Filtek Z350 (ASB), Clearfil SE Bond/Z350 (CF), Adper SE Plus/Z350 (ASEP) and P90 Adhesive System/Filtek P90 (P90) were applied on flat dentin surfaces of 20 third molars (n=5). The restored teeth were sectioned perpendicularly to the bonding interface to obtain sticks (0.8 mm2) to be tested after 24 hours (24 h) and 6 months (6 m) of water storage, in a universal testing machine at 0.5 mm/min. The data was analyzed via two-way Analysis of Variance/Bonferroni post hoc tests at 5% global significance. Results Overall outcomes did not indicate a statistical difference for the resin systems (p=0.26) nor time (p=0.62). No interaction between material × time was detected (p=0.28). Mean standard-deviation in MPa at 24 h and 6 m were: ASB 31.38 (4.53) and 30.06 (1.95), CF 34.26 (3.47) and 32.75 (4.18), ASEP 29.54 (4.14) and 33.47 (2.47), P90 30.27 (2.03) and 31.34 (2.19). Conclusions The silorane-based system showed a similar performance to methacrylate-based materials on dentin. All systems were stable in terms of bond strength up to 6 month of water storage.
publisher Faculdade De Odontologia De Bauru - USP
publishDate 2013
url http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1678-77572013000100080
work_keys_str_mv AT sampaiorenatakiritadoi sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
AT wanglinda sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
AT carvalhorodrigovarellade sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
AT garciaeugeniojose sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
AT andradeandreamellode sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
AT kleinjuniorcelsoafonso sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
AT granderosahelenamiranda sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
AT mourasandrakiss sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
_version_ 1756428858370818048