Influence of Water Storage and Bonding Material on Bond Strength of Metallic Brackets to Ceramic

Abstract: This study investigated the influence of water storage (24 h and 6 months), and Transbond XT and Fuji Ortho LC bonding materials on the bond strength of metallic brackets bonded to feldspathic ceramic. Four cylinders of feldspathic ceramic were etched with 10% hydrofluoric acid for 60 s. Each cylinder received two layers of silane. Metallic brackets were bonded to the cylinders using Transbond XT or Fuji Ortho LC. Light-activation was carried out with 40 s total exposure time using Bluephase G2. Half the specimens for each bonding materials (n=20) were stored in distilled water at 37 °C for 24 h and the other half for 6 months. Shear bond strength testing was performed after storage times at a crosshead speed of 1 mm/min. The adhesive remnant index (ARI) was used to evaluate the amount of adhesive remaining on the ceramic surface at ×8 magnification. Data were subjected to two-way ANOVA and Tukey's test (p<0.05). Transbond XT showed significantly higher bond strength (p<0.05) than Fuji Ortho LC. Significant differences in bond strength (p<0.05) were found when 24 h and 6 months storage times were compared between materials. ARI showed a predominance of score 0 for all groups, and higher scores at 1, 2 and 3 for 24 h storage time. In conclusion, storage time and bonding materials showed significant influence on the bond strength of brackets to ceramic.

Saved in:
Bibliographic Details
Main Authors: Costa,Ana Rosa, Correr,Américo Bortolazzo, Consani,Simonides, Giorgi,Maria Cecília Caldas, Vedovello,Silvia Amélia, Vedovello Filho,Mário, Santos,Eduardo Cesar Almada, Correr-Sobrinho,Lourenço
Format: Digital revista
Language:English
Published: Fundação Odontológica de Ribeirão Preto 2015
Online Access:http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0103-64402015000500503
Tags: Add Tag
No Tags, Be the first to tag this record!
id oai:scielo:S0103-64402015000500503
record_format ojs
spelling oai:scielo:S0103-644020150005005032015-12-03Influence of Water Storage and Bonding Material on Bond Strength of Metallic Brackets to CeramicCosta,Ana RosaCorrer,Américo BortolazzoConsani,SimonidesGiorgi,Maria Cecília CaldasVedovello,Silvia AméliaVedovello Filho,MárioSantos,Eduardo Cesar AlmadaCorrer-Sobrinho,Lourenço shear bond strength orthodontic bracket ceramic bonding storage time. Abstract: This study investigated the influence of water storage (24 h and 6 months), and Transbond XT and Fuji Ortho LC bonding materials on the bond strength of metallic brackets bonded to feldspathic ceramic. Four cylinders of feldspathic ceramic were etched with 10% hydrofluoric acid for 60 s. Each cylinder received two layers of silane. Metallic brackets were bonded to the cylinders using Transbond XT or Fuji Ortho LC. Light-activation was carried out with 40 s total exposure time using Bluephase G2. Half the specimens for each bonding materials (n=20) were stored in distilled water at 37 °C for 24 h and the other half for 6 months. Shear bond strength testing was performed after storage times at a crosshead speed of 1 mm/min. The adhesive remnant index (ARI) was used to evaluate the amount of adhesive remaining on the ceramic surface at ×8 magnification. Data were subjected to two-way ANOVA and Tukey's test (p<0.05). Transbond XT showed significantly higher bond strength (p<0.05) than Fuji Ortho LC. Significant differences in bond strength (p<0.05) were found when 24 h and 6 months storage times were compared between materials. ARI showed a predominance of score 0 for all groups, and higher scores at 1, 2 and 3 for 24 h storage time. In conclusion, storage time and bonding materials showed significant influence on the bond strength of brackets to ceramic.info:eu-repo/semantics/openAccessFundação Odontológica de Ribeirão PretoBrazilian Dental Journal v.26 n.5 20152015-10-01info:eu-repo/semantics/articletext/htmlhttp://old.scielo.br/scielo.php?script=sci_arttext&pid=S0103-64402015000500503en10.1590/0103-6440201300403
institution SCIELO
collection OJS
country Brasil
countrycode BR
component Revista
access En linea
databasecode rev-scielo-br
tag revista
region America del Sur
libraryname SciELO
language English
format Digital
author Costa,Ana Rosa
Correr,Américo Bortolazzo
Consani,Simonides
Giorgi,Maria Cecília Caldas
Vedovello,Silvia Amélia
Vedovello Filho,Mário
Santos,Eduardo Cesar Almada
Correr-Sobrinho,Lourenço
spellingShingle Costa,Ana Rosa
Correr,Américo Bortolazzo
Consani,Simonides
Giorgi,Maria Cecília Caldas
Vedovello,Silvia Amélia
Vedovello Filho,Mário
Santos,Eduardo Cesar Almada
Correr-Sobrinho,Lourenço
Influence of Water Storage and Bonding Material on Bond Strength of Metallic Brackets to Ceramic
author_facet Costa,Ana Rosa
Correr,Américo Bortolazzo
Consani,Simonides
Giorgi,Maria Cecília Caldas
Vedovello,Silvia Amélia
Vedovello Filho,Mário
Santos,Eduardo Cesar Almada
Correr-Sobrinho,Lourenço
author_sort Costa,Ana Rosa
title Influence of Water Storage and Bonding Material on Bond Strength of Metallic Brackets to Ceramic
title_short Influence of Water Storage and Bonding Material on Bond Strength of Metallic Brackets to Ceramic
title_full Influence of Water Storage and Bonding Material on Bond Strength of Metallic Brackets to Ceramic
title_fullStr Influence of Water Storage and Bonding Material on Bond Strength of Metallic Brackets to Ceramic
title_full_unstemmed Influence of Water Storage and Bonding Material on Bond Strength of Metallic Brackets to Ceramic
title_sort influence of water storage and bonding material on bond strength of metallic brackets to ceramic
description Abstract: This study investigated the influence of water storage (24 h and 6 months), and Transbond XT and Fuji Ortho LC bonding materials on the bond strength of metallic brackets bonded to feldspathic ceramic. Four cylinders of feldspathic ceramic were etched with 10% hydrofluoric acid for 60 s. Each cylinder received two layers of silane. Metallic brackets were bonded to the cylinders using Transbond XT or Fuji Ortho LC. Light-activation was carried out with 40 s total exposure time using Bluephase G2. Half the specimens for each bonding materials (n=20) were stored in distilled water at 37 °C for 24 h and the other half for 6 months. Shear bond strength testing was performed after storage times at a crosshead speed of 1 mm/min. The adhesive remnant index (ARI) was used to evaluate the amount of adhesive remaining on the ceramic surface at ×8 magnification. Data were subjected to two-way ANOVA and Tukey's test (p<0.05). Transbond XT showed significantly higher bond strength (p<0.05) than Fuji Ortho LC. Significant differences in bond strength (p<0.05) were found when 24 h and 6 months storage times were compared between materials. ARI showed a predominance of score 0 for all groups, and higher scores at 1, 2 and 3 for 24 h storage time. In conclusion, storage time and bonding materials showed significant influence on the bond strength of brackets to ceramic.
publisher Fundação Odontológica de Ribeirão Preto
publishDate 2015
url http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0103-64402015000500503
work_keys_str_mv AT costaanarosa influenceofwaterstorageandbondingmaterialonbondstrengthofmetallicbracketstoceramic
AT correramericobortolazzo influenceofwaterstorageandbondingmaterialonbondstrengthofmetallicbracketstoceramic
AT consanisimonides influenceofwaterstorageandbondingmaterialonbondstrengthofmetallicbracketstoceramic
AT giorgimariaceciliacaldas influenceofwaterstorageandbondingmaterialonbondstrengthofmetallicbracketstoceramic
AT vedovellosilviaamelia influenceofwaterstorageandbondingmaterialonbondstrengthofmetallicbracketstoceramic
AT vedovellofilhomario influenceofwaterstorageandbondingmaterialonbondstrengthofmetallicbracketstoceramic
AT santoseduardocesaralmada influenceofwaterstorageandbondingmaterialonbondstrengthofmetallicbracketstoceramic
AT corrersobrinholourenco influenceofwaterstorageandbondingmaterialonbondstrengthofmetallicbracketstoceramic
_version_ 1756404564067614720