Microstructural evaluation on shape recovery in stainless Fe-Mn-Si-Cr-Ni-Co SMA processed by wire drawing

The effect of the microstructure on the shape recovery in stainless Fe-8Mn-5Si-13Cr-6Ni-12Co shape memory steel (SSMS) was evaluated using tensile tests and reversion temperature of 600ºC for a pre-strain of 4%. The tests were performed for a solution treated and annealed conditions at different temperatures after wire drawing of 57% area reduction. The best total shape recovery (TSR) was 83% for a sample deformed and annealed at 850ºC. It was concluded that the elastic (or, superelastic) shape recovery (ESR) is high when the austenitic matrix strength is high surpassing the value of shape recovery due to memory effect (SR) and once the austenitic matrix becomes softer, the contribution of SR increases and that of ESR decreases.

Saved in:
Bibliographic Details
Main Authors: Andrade,Elaine Cristina, Bernardi,Heide Heloise, Otubo,Jorge
Format: Digital revista
Language:English
Published: ABM, ABC, ABPol 2014
Online Access:http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392014000300007
Tags: Add Tag
No Tags, Be the first to tag this record!
id oai:scielo:S1516-14392014000300007
record_format ojs
spelling oai:scielo:S1516-143920140003000072014-06-18Microstructural evaluation on shape recovery in stainless Fe-Mn-Si-Cr-Ni-Co SMA processed by wire drawingAndrade,Elaine CristinaBernardi,Heide HeloiseOtubo,Jorge Stainless Shape Memory Steel (SSMS) wire drawing microstructure elastic shape recovery memory shape recovery The effect of the microstructure on the shape recovery in stainless Fe-8Mn-5Si-13Cr-6Ni-12Co shape memory steel (SSMS) was evaluated using tensile tests and reversion temperature of 600ºC for a pre-strain of 4%. The tests were performed for a solution treated and annealed conditions at different temperatures after wire drawing of 57% area reduction. The best total shape recovery (TSR) was 83% for a sample deformed and annealed at 850ºC. It was concluded that the elastic (or, superelastic) shape recovery (ESR) is high when the austenitic matrix strength is high surpassing the value of shape recovery due to memory effect (SR) and once the austenitic matrix becomes softer, the contribution of SR increases and that of ESR decreases.info:eu-repo/semantics/openAccessABM, ABC, ABPolMaterials Research v.17 n.3 20142014-06-01info:eu-repo/semantics/articletext/htmlhttp://old.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392014000300007en10.1590/S1516-14392014005000072
institution SCIELO
collection OJS
country Brasil
countrycode BR
component Revista
access En linea
databasecode rev-scielo-br
tag revista
region America del Sur
libraryname SciELO
language English
format Digital
author Andrade,Elaine Cristina
Bernardi,Heide Heloise
Otubo,Jorge
spellingShingle Andrade,Elaine Cristina
Bernardi,Heide Heloise
Otubo,Jorge
Microstructural evaluation on shape recovery in stainless Fe-Mn-Si-Cr-Ni-Co SMA processed by wire drawing
author_facet Andrade,Elaine Cristina
Bernardi,Heide Heloise
Otubo,Jorge
author_sort Andrade,Elaine Cristina
title Microstructural evaluation on shape recovery in stainless Fe-Mn-Si-Cr-Ni-Co SMA processed by wire drawing
title_short Microstructural evaluation on shape recovery in stainless Fe-Mn-Si-Cr-Ni-Co SMA processed by wire drawing
title_full Microstructural evaluation on shape recovery in stainless Fe-Mn-Si-Cr-Ni-Co SMA processed by wire drawing
title_fullStr Microstructural evaluation on shape recovery in stainless Fe-Mn-Si-Cr-Ni-Co SMA processed by wire drawing
title_full_unstemmed Microstructural evaluation on shape recovery in stainless Fe-Mn-Si-Cr-Ni-Co SMA processed by wire drawing
title_sort microstructural evaluation on shape recovery in stainless fe-mn-si-cr-ni-co sma processed by wire drawing
description The effect of the microstructure on the shape recovery in stainless Fe-8Mn-5Si-13Cr-6Ni-12Co shape memory steel (SSMS) was evaluated using tensile tests and reversion temperature of 600ºC for a pre-strain of 4%. The tests were performed for a solution treated and annealed conditions at different temperatures after wire drawing of 57% area reduction. The best total shape recovery (TSR) was 83% for a sample deformed and annealed at 850ºC. It was concluded that the elastic (or, superelastic) shape recovery (ESR) is high when the austenitic matrix strength is high surpassing the value of shape recovery due to memory effect (SR) and once the austenitic matrix becomes softer, the contribution of SR increases and that of ESR decreases.
publisher ABM, ABC, ABPol
publishDate 2014
url http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392014000300007
work_keys_str_mv AT andradeelainecristina microstructuralevaluationonshaperecoveryinstainlessfemnsicrnicosmaprocessedbywiredrawing
AT bernardiheideheloise microstructuralevaluationonshaperecoveryinstainlessfemnsicrnicosmaprocessedbywiredrawing
AT otubojorge microstructuralevaluationonshaperecoveryinstainlessfemnsicrnicosmaprocessedbywiredrawing
_version_ 1756420542877925376