Strength and stiffness of thermally rectified eucalyptus wood under compression

The aim of this work was the evaluation of the thermal-rectification process of reforestation wood Corymbia citriodora Hook by measuring of mechanical properties under compression parallel to the grain and also determining of chemical composition. The tested samples were thermally treated in a furnace with nitrogen-atmosphere at heating rate of 0.033 ºC.min-1, at temperatures of 160, 180, 200, 220 and 240 ºC. The chemical components and mechanical properties were affected with the thermal rectification process. The contents ranged from 17.85 to 3.51% extractives, 30.44 to 53.86% lignin, 69.56 to 46.14% holocellulose and 0.31 to 0.47% ashes. The samples strength decreased from 20% to 50% and the elasticity modulus increased about 47%. The characteristic values of strength under compression were determined and these changes were about 23% lower than Brazilian standard. The best mechanical properties of Corymbia citriodora were obtained at 180 ºC.

Saved in:
Bibliographic Details
Main Authors: Silva,Marcio Rogério da, Machado,Gilmara de Oliveira, Brito,José Otávio, Calil Junior,Carlito
Format: Digital revista
Language:English
Published: ABM, ABC, ABPol 2013
Online Access:http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392013000500018
Tags: Add Tag
No Tags, Be the first to tag this record!